This probably has been covered somewhere but I couldn't find it.
Why for making heat blankets everybody using two parts silicone? Why not use one part silicone in 10oz tubes? Obviously high-temperature kind up to 400°.
Why for making heat blankets everybody using two parts silicone? Why not use one part silicone in 10oz tubes? Obviously high-temperature kind up to 400°.
- MontuckyMadman
- Posts: 2395
- Joined: Fri Jun 20, 2008 9:41 pm
-
- Posts: 712
- Joined: Thu Sep 30, 2010 12:32 pm
- Location: USA
- MontuckyMadman
- Posts: 2395
- Joined: Fri Jun 20, 2008 9:41 pm
the two part stuff I have used is definitely thinner than the stuff you use for caulking, so easier to vaccume bag also, the 2 part will cure with heat, not sure about the 1 part, prolly speed it up but not that much.
2 part most likely has better elongation at break and tear strength, more durable and may bond better with non silicon type materials most likely.
2 part most likely has better elongation at break and tear strength, more durable and may bond better with non silicon type materials most likely.
sammer wrote: I'm still a tang on top guy.
-
- Posts: 712
- Joined: Thu Sep 30, 2010 12:32 pm
- Location: USA
Don't know about elongation at break and tear strength. IMO reinforced with mesh and outer shell it shouldn't make that much difference. Bonding seems like fine in my testMontuckyMadman wrote:the two part stuff I have used is definitely thinner than the stuff you use for caulking, so easier to vaccume bag also, the 2 part will cure with heat, not sure about the 1 part, prolly speed it up but not that much.
2 part most likely has better elongation at break and tear strength, more durable and may bond better with non silicon type materials most likely.
-
- Posts: 217
- Joined: Sun Jan 22, 2012 10:03 pm
- Location: The Dalles Oregon
-
- Posts: 712
- Joined: Thu Sep 30, 2010 12:32 pm
- Location: USA
If cost number one reason then 10oz tubes cheaper for me and don't need to be shipped.troublemaker wrote:Cost is number one, you can get a 9 pound tub of two part for $80 shipped enough for 3 heat mats. Silcone in a tube feels kinda wierd once cured.
I checked another day commercially made blanket it need very little of silicon just enough to hold all components together not even 1/16" thickness
-
- Posts: 217
- Joined: Sun Jan 22, 2012 10:03 pm
- Location: The Dalles Oregon
-
- Posts: 712
- Joined: Thu Sep 30, 2010 12:32 pm
- Location: USA
Obviously I'm not talking retail pricetroublemaker wrote:I tried using tubes of silicone from the auto parts store once, seemed like they were about $10 per tube. The stuff in the tubes would probably work with the material you sent me. If you were to build the whole mat out of the tubes I think it would be really hard to spread out evenly.
Yes it will be challenge to make silicone smooth especially do it all in one shot. If I have to guess before making some small-scale trials. Should be 2 or 3 steps with silicone drying in between to make it all works. I done some plaster and cement work this shouldn't be that much different. Need practice a little