exactly my point. could create more problems than that supposed to solve.Akiwi wrote:I used a hot box for a 2 component clear coat, and it developed bubbles. A right p.i.t.a. Couldn't get rid of them. Ruined a good project.
Probably you overheat it. I had something similar on one of the tests I did. PU start looks like boiling
For now I got decent results with normal eight hours lol drying. If anything will try post cure heating to accelerate full cure and that don't require anything additional to make